Influence of sulfate ion on fluoride removal from flue gas scrubbing wastewater using lanthanum salts
Xiao-cong ZHONG1,2,3, Chen CHEN1, Kang YAN1,2, Kui-fang ZHANG1,4, Rui-xiang WANG1,3, Zhi-feng XU2

1. Faculty of Materials Metallurgy and Chemistry, Jiangxi University of Science and Technology, Ganzhou 341000, China;
2. Key Laboratory of Ionic Rare Earth Resources and Environment, Ministry of Natural Resources, Ganzhou 341000, China;
3. Ganzhou Engineering Technology Research Center of Green Metallurgy and Process Intensification, Ganzhou 341000, China;
4. Institute of Resources Utilization and Rare Earth Development, Guangdong Academy of Sciences, Guangzhou 510650, China

Abstract:Batch experiments were conducted to remove fluoride from simulated flue-gas scrubbing wastewater using La(NO3)3·6H2O. The effects of SO42- concentration and addition sequence on residual fluoride concentration and precipitates properties (mass, morphology, phase structure and composition) were investigated using fluorine ion-selective electrode, SEM, EDS and XRD. The results show that precipitates obtained in the presence of SO42- mainly consisted of LaF3 in irregular bulk shape with high crystallinity. However, amorphous particles were observed in the precipitates, which were speculated to be La[SO4]F. Due to the smaller stoichiometric coefficient of F/La in La[SO4]F compared to that in LaF3, the residual fluoride concentration increased as the SO42- concentration ascended. Subsequent addition of SO42- after lanthanum salt could inhibit the formation of amorphous particles, and further reduce the residual fluoride concentration. At a La/F molar ratio of 1:3.0, the subsequent addition of SO42- (0.02 mol/L) after La(NO3)3?6H2O could obtain a residual fluoride concentration of 6.9 mg/L, lower than the required fluoride emission level. Further increasing the La/F molar ratio could reduce residual fluoride concentration to below 2 mg/L, while the risk of retaining La3+ would emerge.

 

Key words: fluoride removal; lanthanum salts; amorphous particles; atomic efficiency; addition sequence

ISSN 1004-0609
CN 43-1238/TG
CODEN: ZYJXFK

ISSN 1003-6326
CN 43-1239/TG
CODEN: TNMCEW

主管:中國科學技術協(xié)會 主辦:中國有色金屬學會 承辦:中南大學
湘ICP備09001153號 版權所有:《中國有色金屬學報》編輯部
------------------------------------------------------------------------------------------
地 址:湖南省長沙市岳麓山中南大學內 郵編:410083
電 話:0731-88876765,88877197,88830410   傳真:0731-88877197   電子郵箱:f_ysxb@163.com  
方山县| 乌苏市| 乐安县| 措勤县| 扎兰屯市| 三明市| 五大连池市| 浠水县| 田阳县| 湖口县| 河北省| 八宿县| 湖南省| 正蓝旗| 滁州市| 裕民县| 永州市| 舟山市| 张家口市| 仁布县| 邢台县| 乌拉特后旗| 台南县| 团风县| 循化| 平湖市| 南投市| 铜川市| 滕州市| 尼勒克县| 平陆县| 科技| 大安市| 仙桃市| 奉贤区| 正定县| 张家界市| 林周县| 伊宁县| 静安区| 开平市|